Effect of temperature on tensile behavior of Ni–Cr–W based superalloy
Guanghai Bai, Jinshan Li, Rui Hu, Zengwu Tang, Xiangyi Xue, Hengzhi FuVolume:
528
Year:
2011
Language:
english
Pages:
5
DOI:
10.1016/j.msea.2010.11.053
File:
PDF, 1.01 MB