![](/img/cover-not-exists.png)
Optimising a multipass arc welding procedure
Galopin, M, Laroche, Y, Coté, J L, Boillot, J PVolume:
5
Language:
english
Journal:
Welding International
DOI:
10.1080/09507119109447833
Date:
January, 1991
File:
PDF, 1.55 MB
english, 1991