![](/img/cover-not-exists.png)
Assessment of elastic anisotropy and incipient plasticity in Fe3C by nanoindentation
Alkorta, Jon, Sevillano, Javier GilVolume:
27
Language:
english
Journal:
Journal of Materials Research
DOI:
10.1557/jmr.2011.284
Date:
January, 2012
File:
PDF, 357 KB
english, 2012