On the Mechanical Properties of Transversely Isotropic Material Using the Nanoindentation
Ko, Seong Hyun, Kim, Young Deuk, Shin, Na Young, Park, Hyun Chul, Lee, Kun HongVolume:
33-37
Year:
2008
Language:
english
Journal:
Advanced Materials Research
DOI:
10.4028/www.scientific.net/AMR.33-37.987
File:
PDF, 3.15 MB
english, 2008