Nickel based superalloy welding practices for industrial gas turbine applications
Henderson, M. B., Arrell, D., Larsson, R., Heobel, M., Marchant, G.Volume:
9
Language:
english
Journal:
Science and Technology of Welding and Joining
DOI:
10.1179/136217104225017099
Date:
February, 2004
File:
PDF, 1.18 MB
english, 2004