![](/img/cover-not-exists.png)
A Study on the Nanoindentation Behaviour of Single Crystal Silicon Using Hybrid MD-FE Method
Khatibi, Akbar Afaghi, Mortazavi, BohayraVolume:
32
Year:
2008
Language:
english
Journal:
Advanced Materials Research
DOI:
10.4028/www.scientific.net/AMR.32.259
File:
PDF, 402 KB
english, 2008