![](/img/cover-not-exists.png)
The Solidification Microstructure and Carbide Formation Behaviors in the Cobalt-Based Superalloy ECY768
Lee, J.S., Lee, Je Hyun, Choi, Baig Gyu, Jo, Chang Yong, Paik, Un Gyu, Gang, S.G.Volume:
486-487
Year:
2005
Language:
english
Journal:
Materials Science Forum
DOI:
10.4028/www.scientific.net/MSF.486-487.374
File:
PDF, 1.93 MB