Orientation Relationship of Phases in an Oxidation Protection Coating on a Ni-Based Superalloy Single Crystal
Zaefferer, Stefan, Glatzel, UweVolume:
408-412
Year:
2002
Journal:
Materials Science Forum
DOI:
10.4028/www.scientific.net/MSF.408-412.1531
File:
PDF, 676 KB