Isothermal and Cyclic Oxidation of Chromia Forming Nickel-Based Superalloys
Chen, J.H., Rogers, P.M., Little, J.A.Volume:
251-254
Year:
1997
Language:
english
Journal:
Materials Science Forum
DOI:
10.4028/www.scientific.net/MSF.251-254.57