Atomic Layer Deposition of Inverse Opals for Solar Cell Applications
Karuturi, Siva Krishna, Liu, Li Jun, Su, Liap Tat, Niu, Wen Bin, Tok, Alfred Ling YoongVolume:
789
Language:
english
Journal:
Advanced Materials Research
DOI:
10.4028/www.scientific.net/AMR.789.3
Date:
September, 2013
File:
PDF, 633 KB
english, 2013