Mechanical properties of plasma polymer film evaluated by conventional and alternative nanoindentation techniques
R. Trivedi, V. CechVolume:
205
Year:
2010
Language:
english
Pages:
1
DOI:
10.1016/j.surfcoat.2010.08.002
File:
PDF, 282 KB
english, 2010