![](/img/cover-not-exists.png)
H-bonding in entrapped water in poly(o-methoxyaniline): Results from a differential scanning calorimetry study
Nara C. de Souza, Josmary R. Silva, José A. Giacometti, Osvaldo N. Oliveira Jr.Volume:
441
Year:
2006
Language:
english
Pages:
3
DOI:
10.1016/j.tca.2005.12.016
File:
PDF, 163 KB
english, 2006