![](/img/cover-not-exists.png)
Characterization of Precipitation Kinetics of Inconel 718 Superalloy by the Stress Relaxation Technique
Calvo, Jessica, Shu, She Yu, Cabrera, Jose MariaVolume:
706-709
Language:
english
Journal:
Materials Science Forum
DOI:
10.4028/www.scientific.net/MSF.706-709.2393
Date:
January, 2012
File:
PDF, 5.38 MB