Intergranular and Pitting Corrosion Behavior of Fe-25Al-6Cr Intermetallic Compounds Containing Mo, Nb and B
Choe, Han Cheol, Park, S.J., Eun, S.W., Ko, Yeong MuVolume:
539-543
Year:
2007
Language:
english
Journal:
Materials Science Forum
DOI:
10.4028/www.scientific.net/MSF.539-543.1583
File:
PDF, 780 KB