![](/img/cover-not-exists.png)
Cracking susceptibility after post-weld heat treatment in Haynes 282 nickel based superalloy
Osoba, L. O., Khan, A. K., Adeosun, S. O.Volume:
26
Language:
english
Journal:
Acta Metallurgica Sinica (English Letters)
DOI:
10.1007/s40195-013-0252-3
Date:
December, 2013
File:
PDF, 1.16 MB
english, 2013