![](/img/cover-not-exists.png)
Microstructural Characterization and Pitting Corrosion Behavior of UNS S30466 Borated Stainless Steel
Moreno, D. A., Molina, B., Ranninger, C., Montero, F., Izquierdo, J.Volume:
60
Language:
english
Journal:
Corrosion
DOI:
10.5006/1.3287761
Date:
June, 2004
File:
PDF, 834 KB
english, 2004