Study of mechanical properties of light-emitting polymer films by nano-indentation technique
Kaiyang Zeng, Zhi-Kuan Chen, Lu Shen, Bin LiuVolume:
477
Year:
2005
Language:
english
Pages:
8
DOI:
10.1016/j.tsf.2004.08.119
File:
PDF, 203 KB