![](/img/cover-not-exists.png)
Finite Element Simulation and Optimisation of Ageing Precipitation in Nickel Base Superalloys with a Low Gamma-Prime (g’) Volume Fraction
Tancret, Franck, Guillemet, Philippe, Fournier Dit Chabert, Florent, Le Gall, René, Castagné, Jean FrançoisVolume:
172-174
Language:
english
Journal:
Solid State Phenomena
DOI:
10.4028/www.scientific.net/SSP.172-174.881
Date:
June, 2011
File:
PDF, 330 KB
english, 2011