![](/img/cover-not-exists.png)
Statistical Analysis of Pitting Corrosion Field Data and Their Use for Realistic Reliability Estimations in Non-Piggable Pipeline Systems
Valor, Alma, Caleyo, Francisco, Alfonso, Lester, Vidal, Julio, Hallen, José M.Volume:
70
Language:
english
Journal:
Corrosion
DOI:
10.5006/1195
Date:
November, 2014
File:
PDF, 1.49 MB