![](/img/cover-not-exists.png)
Influence of Potential and pH on the Stress Corrosion Cracking of a Duplex Stainless Steel in Chloride Solution
Ghosal, S.K., De, P.K., Gadiyar, H.S., Prabhugaonkar, G.V.Volume:
20-28
Language:
english
Journal:
Key Engineering Materials
DOI:
10.4028/www.scientific.net/KEM.20-28.2223
Date:
January, 1991
File:
PDF, 5.56 MB
english, 1991