![](/img/cover-not-exists.png)
Variations of Internal Stresses within a Rafted Superalloy during High Temperature Mechanical Testing: An in situ XRD Study
Jacques, Alain, Dirand, Laura, Schenk, Thomas, Chateau-Cornu, Jean Philippe, Ferry, Olivier, Bastie, PierreVolume:
1528
Language:
english
Journal:
MRS Proceedings
DOI:
10.1557/opl.2013.365
Date:
January, 2013
File:
PDF, 4.61 MB
english, 2013