![](/img/cover-not-exists.png)
Linear Friction Welding of a Single Crystal Superalloy
Wanjara, Priti, Dalgaard, Elvi, Gholipour, Javad, Larose, JoelVolume:
706-709
Language:
english
Journal:
Materials Science Forum
DOI:
10.4028/www.scientific.net/MSF.706-709.3022
Date:
January, 2012
File:
PDF, 7.65 MB
english, 2012