Experimental Investigation on Micro Electrochemical Milling of Nickel-Based Superalloy
Liu, Yong, Zeng, Yong BinVolume:
229-231
Language:
english
Journal:
Applied Mechanics and Materials
DOI:
10.4028/www.scientific.net/AMM.229-231.2436
Date:
November, 2012