Studies of Nanomechanical Properties of Pulsed Laser Deposited NbN films on Si Using Nanoindentation
Mamun, M. A., Farha, A. H., Ufuktepe, Y., Elsayed-Ali, H. E., Elmustafa, A. A.Volume:
1424
Language:
english
Journal:
MRS Proceedings
DOI:
10.1557/opl.2012.152
Date:
January, 2012