![](/img/cover-not-exists.png)
Study on capacity fade factors of lithium secondary batteries using LiNi0.7Co0.3O2 and graphite–coke hybrid carbon
Yoshinori Kida, Akira Kinoshita, Katsunori Yanagida, Atsuhiro Funahashi, Toshiyuki Nohma, Ikuo YonezuVolume:
47
Year:
2002
Language:
english
Pages:
6
DOI:
10.1016/s0013-4686(02)00371-7
File:
PDF, 255 KB
english, 2002