![](/img/cover-not-exists.png)
Computer Program Set for Superplastic Material Creep Test Simulation
Miad, A.R., Tsepin, M.A., Yershov, A.N.Volume:
170-172
Year:
1994
Journal:
Materials Science Forum
DOI:
10.4028/www.scientific.net/MSF.170-172.663
File:
PDF, 357 KB
1994