![](/img/cover-not-exists.png)
Nanoindentation Applied to Materials with an Inner Structure
Němeček, JiříVolume:
586
Language:
english
Journal:
Key Engineering Materials
DOI:
10.4028/www.scientific.net/kem.586.55
Date:
September, 2013
File:
PDF, 399 KB
english, 2013