![](/img/cover-not-exists.png)
Review of Models to Predict Internal Pitting Corrosion Of Oil and Gas Pipelines
Papavinasam, Sankara, Revie, R.Winston, I.Friesen, Waldemar, Doiron, Alex, Panneerselvan, TharaniVolume:
24
Language:
english
Journal:
Corrosion Reviews
DOI:
10.1515/CORRREV.2006.24.3-4.173
Date:
January, 2006
File:
PDF, 5.00 MB
english, 2006