![](/img/cover-not-exists.png)
Cyclic oxidation behavior of Cr-/Si-modified NiAlHf coatings on single-crystal superalloy produced by EB-PVD
Lu Wang,Lu-Lu Pan,Hui Peng,Hong-Bo Guo,Sheng-Kai GongVolume:
35
Language:
english
Journal:
Rare Metals
DOI:
10.1007/s12598-015-0482-9
Date:
May, 2016
File:
PDF, 1.55 MB
english, 2016