X-ray microtomography studies of localised corrosion and transitions to stress corrosion cracking
Connolly, B. J., Horner, D. A., Fox, S. J., Davenport, A. J., Padovani, C., Zhou, S., Turnbull, A., Preuss, M., Stevens, N. P., Marrow, T. J., Buffiere, J.-Y., Boller, E., Groso, A., Stampanoni, M.Volume:
22
Language:
english
Journal:
Materials Science and Technology
DOI:
10.1179/174328406x114199
Date:
September, 2006
File:
PDF, 616 KB
english, 2006