Formation of low angle boundaries in Ni-based superalloys
Newell, M., D'Souza, N., Green, N. R.Volume:
22
Language:
english
Journal:
International Journal of Cast Metals Research
DOI:
10.1179/136404609X367353
Date:
August, 2009
File:
PDF, 265 KB
english, 2009