Differential scanning calorimetry evaluation of autoclaved cement based building materials made with construction and demolition waste
Danielle S. Klimesch, Abhi Ray, Jean-Pierre GuerboisVolume:
389
Year:
2002
Language:
english
Pages:
4
DOI:
10.1016/s0040-6031(02)00058-8
File:
PDF, 84 KB
english, 2002