![](/img/cover-not-exists.png)
Elastic constant measurement of Ni-base superalloy with the RUS and mode selective EMAR methods
Tetsu Ichitsubo, Hirotsugu Ogi, Masahiko Hirao, Katsushi Tanaka, Makoto Osawa, Tadaharu Yokokawa, Toshiharu Kobayashi, Hiroshi HaradaVolume:
40
Year:
2002
Language:
english
Pages:
5
DOI:
10.1016/s0041-624x(02)00139-7
File:
PDF, 158 KB