![](/img/cover-not-exists.png)
Fractographic Analysis of Flexural Failures in Thermally Aged APC-2 Laminates
Carew, A., Buggy, MartinVolume:
72-74
Year:
1992
Language:
english
Journal:
Key Engineering Materials
DOI:
10.4028/www.scientific.net/KEM.72-74.653
File:
PDF, 670 KB
english, 1992