![](/img/cover-not-exists.png)
Electrical Discharge Machining of René 108 DS Nickel Superalloy for Aerospace Turbine Blades
Caiazzo, Fabrizia, Cuccaro, Luigi, Fierro, Ilaria, Petrone, Giuseppe, Alfieri, VittorioVolume:
33
Year:
2015
Language:
english
Journal:
Procedia CIRP
DOI:
10.1016/j.procir.2015.06.086
File:
PDF, 563 KB