Atomic layer deposition of biobased nanostructured interfaces for energy, environmental and health applications
Bechelany, Mikhael, Balme, Sebastien, Miele, PhilippeVolume:
87
Language:
english
Journal:
Pure and Applied Chemistry
DOI:
10.1515/pac-2015-0102
Date:
January, 2015