Fatigue crack propagation in a ductile superalloy at room temperature and extensive cyclic plastic flow
Ewest, D., Almroth, P., Leidermark, D., Simonsson, K., Sjödin, B.Volume:
80
Language:
english
Journal:
International Journal of Fatigue
DOI:
10.1016/j.ijfatigue.2015.04.006
Date:
November, 2015
File:
PDF, 2.04 MB
english, 2015