Low cycle fatigue properties and microstructure evolution at 760°C of a single crystal superalloy
Shi, Zhenxue, Wang, Xiaoguang, Liu, Shizhong, Li, JiarongVolume:
25
Language:
english
Journal:
Progress in Natural Science: Materials International
DOI:
10.1016/j.pnsc.2015.01.009
Date:
February, 2015
File:
PDF, 4.49 MB
english, 2015