![](/img/cover-not-exists.png)
Theory on the Thermoanalytical Techniques in Differential Scanning Calorimetry. Application to the Crystallization of the Semiconducting Sb 0.20 As 0.32 Se 0.48 Alloy
Vázquez, J, González-Palma, R, López-Alemany, P L, Villares, P, Jiménez-Garay, RVolume:
72
Language:
english
Journal:
Physica Scripta
DOI:
10.1238/Physica.Regular.072a00258
Date:
January, 2005
File:
PDF, 230 KB
english, 2005