An international round-robin experiment to evaluate the consistency of nanoindentation hardness measurements of thin films
Kitty W Lee, Yip-Wah Chung, C.Y Chan, I Bello, S.T Lee, Ayatollah Karimi, Joerg Patscheider, M.P Delplancke-Ogletree, Dehua Yang, Brad Boyce, Thomas BuchheitVolume:
168