A gel-derived mesoporous silica reference material for surface analysis by gas sorption 1. Textural features
N.J. Coleman, L.L. HenchVolume:
26
Year:
2000
Language:
english
Pages:
8
DOI:
10.1016/s0272-8842(99)00037-1