Electronic structure of the γ'+γ phase in nickel-based superalloys
Cao, Junchu, Liu, Fu-sui, Wang, Chong-yuVolume:
18
Language:
english
Journal:
Journal of Physics F: Metal Physics
DOI:
10.1088/0305-4608/18/8/019
Date:
August, 1988
File:
PDF, 434 KB
english, 1988