Atomic layer deposition on 2D transition metal chalcogenides: layer dependent reactivity and seeding with organic ad-layers
Wirtz, Christian, Hallam, Toby, Cullen, Conor Patrick, Berner, Nina C., O'Brien, Maria, Marcia, Mario, Hirsch, Andreas, Duesberg, Georg S.Year:
2015
Language:
english
Journal:
Chem. Commun.
DOI:
10.1039/C5CC05726D