![](/img/cover-not-exists.png)
Decorrelated Dislocation Movement in the γ-Matrix Channels of a Ni-Based Superalloy: Experiment and Dislocation Dynamics Simulation
Pettinari-Sturmel, Florence, Douin, Joël, Locq, Didier, Caron, Pierre, Coujou, ArmandVolume:
278
Journal:
Advanced Materials Research
DOI:
10.4028/www.scientific.net/AMR.278.13
Date:
July, 2011
File:
PDF, 950 KB
2011