![](/img/cover-not-exists.png)
Inhibition of Stress Corrosion Cracking of Type 403 Stainless Steel in Sodium Sulfate Solutions
Bavarian, Behzad, Moccari, Ahmad, Macdonald, Digby D.Volume:
38
Language:
english
Journal:
Corrosion
DOI:
10.5006/1.3577323
Date:
February, 1982
File:
PDF, 9.18 MB
english, 1982