![](/img/cover-not-exists.png)
Relationships Between Pitting, Stress, and Stress Corrosion Cracking of Line Pipe Steels
Christman, T. K.Volume:
46
Language:
english
Journal:
Corrosion
DOI:
10.5006/1.3585131
Date:
June, 1990
File:
PDF, 897 KB
english, 1990