Selective atomic layer deposition onto directly transferred monolayer graphene
Kim, Jangheon, Kim, Soohyun, Jung, WonsukLanguage:
english
Journal:
Materials Letters
DOI:
10.1016/j.matlet.2015.11.111
Date:
November, 2015
File:
PDF, 1.20 MB
english, 2015