![](/img/cover-not-exists.png)
Effect of cold deformation on pitting corrosion of 00Cr18Mn15Mo2N0.86 stainless steel for coronary stent application
Ren, Yibin, Zhao, Haochuan, Liu, Wenpeng, Yang, KeLanguage:
english
Journal:
Materials Science and Engineering: C
DOI:
10.1016/j.msec.2015.11.048
Date:
November, 2015
File:
PDF, 661 KB
english, 2015