Fractography of in-Service Fracture of the Metal in Weld...

Fractography of in-Service Fracture of the Metal in Weld Joint No. 111 of the Steam Generator of a WWER-1000 Power Unit

Krasovskii, A. Ya., Orynyak, I. V., Gopkalo, E. E., Bogdan, A. V., Makovetskaya, I. A.