![](/img/cover-not-exists.png)
Evaluation of friction stresses in the γ phase of a nickel-base superalloy ‘In situ’ deformation experiments
M. Jouiad, F. Pettinari, A. Coujou, N. ClémentVolume:
234-236
Year:
1997
Language:
english
Pages:
4
DOI:
10.1016/s0921-5093(97)00332-8
File:
PDF, 353 KB
english, 1997